The aim of this research was to fabricate and evaluate polyglycerol sebacate/polycaprolactone/reduced graphene oxide (PGS-PCL-RGO) composite scaffolds for myocardial tissue engineering. Polyglycerol sebacate polymer was synthesized using glycerol and sebacic acid prepolymers, confirmed by Fourier-transform infrared spectroscopy (FTIR) and X-ray diffraction (XRD). Six PGS-PCL-RGO composite scaffolds (S-S) with various weight ratios were prepared in chloroform (CF) and acetone (Ace) solvents at 8 CF:2Ace and 9 CF:1Ace volume ratios, using the electrospinning method at a rate of 1 ml/h and a voltage of 18 kV. The scaffolds' chemical composition and microstructure were characterized by FTIR, XRD, and scanning electron microscopy (SEM). Further investigations included tensile testing, contact angle testing, four-point probe testing for electrical conductivity, degradation testing, and cytotoxicity testing (MTT). The results showed that adding 2%wt RGO to the composite scaffold decreased fiber diameter and degradation rate, while increasing electrical conductivity and ductility. The 33%PGS-65%PCL-2%RGO (S) composite scaffold exhibited the lowest degradation rate (23.87 % over 60 days) and the highest electrical conductivity (51E-3 S/m). Mechanical evaluations revealed an elastic modulus of 2.46 MPa and elongation of 62.43 %, aligning closely with the heart muscle's elastomeric properties. The contact angle test indicated that the scaffold was hydrophilic, with a water contact angle of 61 ± 2°. Additionally, the cell toxicity test confirmed that scaffolds containing RGO were non-toxic and supported good cell viability. In conclusion, the 33%PGS-65%PCL-2%RGO composite scaffold exhibits mechanical and structural properties similar to heart tissue, making it an ideal candidate for myocardial tissue engineering.

References
1.
Sant S, Iyer D, Gaharwar A, Patel A, Khademhosseini A . Effect of biodegradation and de novo matrix synthesis on the mechanical properties of valvular interstitial cell-seeded polyglycerol sebacate-polycaprolactone scaffolds. Acta Biomater. 2012; 9(4):5963-73. PMC: 3662231. DOI: 10.1016/j.actbio.2012.11.014. View

2.
Muylaert D, Fledderus J, Bouten C, Dankers P, Verhaar M . Combining tissue repair and tissue engineering; bioactivating implantable cell-free vascular scaffolds. Heart. 2014; 100(23):1825-30. DOI: 10.1136/heartjnl-2014-306092. View

3.
Kerativitayanan P, Gaharwar A . Elastomeric and mechanically stiff nanocomposites from poly(glycerol sebacate) and bioactive nanosilicates. Acta Biomater. 2015; 26:34-44. DOI: 10.1016/j.actbio.2015.08.025. View

4.
Gerlier D, Thomasset N . Use of MTT colorimetric assay to measure cell activation. J Immunol Methods. 1986; 94(1-2):57-63. DOI: 10.1016/0022-1759(86)90215-2. View

5.
Rai R, Tallawi M, Frati C, Falco A, Gervasi A, Quaini F . Bioactive electrospun fibers of poly(glycerol sebacate) and poly(ε-caprolactone) for cardiac patch application. Adv Healthc Mater. 2015; 4(13):2012-25. DOI: 10.1002/adhm.201500154. View