Scenarios and Methods That Induce Protruding or Released CNTs After Degradation of Nanocomposite Materials

Overview
Journal J Nanopart Res
Date 2013 Apr 19
PMID 23596358
Citations 17
Authors
Affiliations
Soon will be listed here.
Abstract

Abstract: Nanocomposite materials may be considered as a low-risk application of nanotechnology, if the nanofillers remain embedded throughout the life-cycle of the products in which they are embedded. We hypothesize that release of free CNTs occurs by a combination of mechanical stress and chemical degradation of the polymer matrix. We experimentally address limiting cases: Mechanically released fragments may show tubular protrusions on their surface. Here we identify these protrusions unambiguously as naked CNTs by chemically resolved microscopy and a suitable preparation protocol. By size-selective quantification of fragments we establish as a lower limit that at least 95 % of the CNTs remain embedded. Contrary to classical fiber composite approaches, we link this phenomenon to matrix materials with only a few percent elongation at break, predicting which materials should still cover their CNT nanofillers after machining. Protruding networks of CNTs remain after photochemical degradation of the matrix, and we show that it takes the worst case combinations of weathering plus high-shear wear to release free CNTs in the order of mg/m/year. Synergy of chemical degradation and mechanical energy input is identified as the priority scenario of CNT release, but its lab simulation by combined methods is still far from real-world validation.

Graphical Abstract:

Citing Articles

Characterization of aerosolized particles from nanoclay-enabled composites during manipulation processes.

Lee E, Cena L, Kwon J, Afshari A, Park H, Casuccio G Environ Sci Nano. 2023; 7:1539-1553.

PMID: 37205161 PMC: 10190203. DOI: 10.1039/c9en01211g.


Quantifying Mechanical Abrasion of MWCNT Nanocomposites Used in 3D Printing: Influence of CNT Content on Abrasion Products and Rate of Microplastic Production.

Bossa N, Sipe J, Berger W, Scott K, Kennedy A, Thomas T Environ Sci Technol. 2021; 55(15):10332-10342.

PMID: 34264058 PMC: 10084403. DOI: 10.1021/acs.est.0c02015.


Occupational Exposure to Carbon Nanotubes and Carbon Nanofibres: More Than a Cobweb.

Bergamaschi E, Garzaro G, Wilson Jones G, Buglisi M, Caniglia M, Godono A Nanomaterials (Basel). 2021; 11(3).

PMID: 33809629 PMC: 8002294. DOI: 10.3390/nano11030745.


Fragmentation of polymer nanocomposites: modulation by dry and wet weathering, fractionation, and nanomaterial filler.

Zepp R, Ruggiero E, Acrey B, Davis M, Han C, Hsieh H Environ Sci Nano. 2021; 7(6):1742-1758.

PMID: 33564464 PMC: 7869489. DOI: 10.1039/c9en01360a.


The Impacts of Moisture and Ultraviolet Light on the Degradation of Graphene Oxide/Polymer Nanocomposites.

Goodwin Jr D, Lai T, Lyu Y, Lu C, Campos A, Reipa V NanoImpact. 2021; 19.

PMID: 33506141 PMC: 7836096. DOI: 10.1016/j.impact.2020.100249.


References
1.
Schlagenhauf L, Chu B, Buha J, Nuesch F, Wang J . Release of carbon nanotubes from an epoxy-based nanocomposite during an abrasion process. Environ Sci Technol. 2012; 46(13):7366-72. DOI: 10.1021/es300320y. View

2.
Yu , Lourie , Dyer , Moloni , Kelly , Ruoff . Strength and breaking mechanism of multiwalled carbon nanotubes under tensile load. Science. 2000; 287(5453):637-40. DOI: 10.1126/science.287.5453.637. View

3.
Raynor P, Cebula J, Spangenberger J, Olson B, Dasch J, DArcy J . Assessing potential nanoparticle release during nanocomposite shredding using direct-reading instruments. J Occup Environ Hyg. 2011; 9(1):1-13. DOI: 10.1080/15459624.2012.633061. View

4.
Poland C, Duffin R, Kinloch I, Maynard A, Wallace W, Seaton A . Carbon nanotubes introduced into the abdominal cavity of mice show asbestos-like pathogenicity in a pilot study. Nat Nanotechnol. 2008; 3(7):423-8. DOI: 10.1038/nnano.2008.111. View

5.
Liu X, Hurt R, Kane A . Biodurability of Single-Walled Carbon Nanotubes Depends on Surface Functionalization. Carbon N Y. 2010; 48(7):1961-1969. PMC: 2844903. DOI: 10.1016/j.carbon.2010.02.002. View