Initial in Vivo Tear Protein Deposition on Individual Hydrogel Contact Lenses

Overview
Journal Optom Vis Sci
Date 1990 Jul 1
PMID 2205814
Citations 7
Authors
Affiliations
Soon will be listed here.
Abstract

We investigated and compared the initial composition, morphology, and time course of deposits on individual soft contact lenses of different water contents and surface charges in order to evaluate the potential for antigenic reactions and to predict the optimal frequency of lens replacement. Newly manufactured lenses were worn for graduated periods of time from 1 min to 8 h by subjects who were first adapted to daily wear soft lenses. The morphology and composition of the deposits were analyzed by histological staining, light microscopy, scanning electron microscopy (SEM), sodium dodecyl sulfate polyacrylamide gel electrophoresis (SDS-PAGE) with silver nitrate staining, and immunofluorescence microscopy. The protein bands of the acrylamide gels were divided according to their molecular weights into six groups which have been defined in the literature from tear analyses by electrophoretic techniques and include lysozyme, proteins migrating faster than albumin (PMFA), protein G, albumin, lactoferrin, and other proteins heavier than albumin such as Ig-G and secretory Ig-A. Specific proteins (lysozyme, PMFA, and protein G) were detected on individual lenses after as little as 1 min of wear. There was an increasing amount of protein deposited as the wearing time increased. Differences in the rates and amounts of deposition were more dependent on lens water content and ionic characteristics than on intersubject differences. Such early significant protein deposition may occur in wearers of disposable lenses as well as in those subject to complications due to accumulation of protein.

Citing Articles

Mechanisms, imaging and structure of tear film breakup.

King-Smith P, Begley C, Braun R Ocul Surf. 2017; 16(1):4-30.

PMID: 28935579 PMC: 5756679. DOI: 10.1016/j.jtos.2017.09.007.


Influence of Tear Protein Deposition on the Oxygen Permeability of Soft Contact Lenses.

Lee S, Kim S, Park M J Ophthalmol. 2017; 2017:5131764.

PMID: 28280635 PMC: 5322617. DOI: 10.1155/2017/5131764.


Corneal cell adhesion to contact lens hydrogel materials enhanced via tear film protein deposition.

Elkins C, Qi Q, Fuller G PLoS One. 2014; 9(8):e105512.

PMID: 25144576 PMC: 4140805. DOI: 10.1371/journal.pone.0105512.


Deposit buildup on prosthetic eyes and implications for conjunctival inflammation and mucoid discharge.

Pine K, Sloan B, Jacobs R Clin Ophthalmol. 2012; 6:1755-62.

PMID: 23152653 PMC: 3497451. DOI: 10.2147/OPTH.S37250.


Composition of incubation solution impacts in vitro protein uptake to silicone hydrogel contact lenses.

Jadi S, Heynen M, Luensmann D, Jones L Mol Vis. 2012; 18:337-47.

PMID: 22355245 PMC: 3283214.