Fast Li-Ion Insertion into Nanosized LiMn(2)O(4) Without Domain Boundaries
Overview
Authors
Affiliations
The effect of crystallite size on Li-ion insertion in electrode materials is of great interest recently because of the need for nanoelectrodes in higher-power Li-ion rechargeable batteries. We present a systematic study of the effect of size on the electrochemical properties of LiMn(2)O(4). Accurate size control of nanocrystalline LiMn(2)O(4), which is realized by a hydrothermal method, significantly alters the phase diagram as well as Li-ion insertion voltage. Nanocrystalline LiMn(2)O(4) with extremely small crystallite size of 15 nm cannot accommodate domain boundaries between Li-rich and Li-poor phases due to interface energy, and therefore lithiation proceeds via solid solution state without domain boundaries, enabling fast Li-ion insertion during the entire discharge process.
A Practical and Sustainable Ni/Co-Free High-Energy Electrode Material: Nanostructured LiMnO.
Miyaoka Y, Sato T, Oguro Y, Kondo S, Nakano K, Nakayama M ACS Cent Sci. 2024; 10(9):1718-1732.
PMID: 39345817 PMC: 11428382. DOI: 10.1021/acscentsci.4c00578.
Earth-abundant Li-ion cathode materials with nanoengineered microstructures.
Hau H, Mishra T, Ophus C, Huang T, Bustilo K, Sun Y Nat Nanotechnol. 2024; 19(12):1831-1839.
PMID: 39300225 PMC: 11638071. DOI: 10.1038/s41565-024-01787-y.
Ex Situ Raman Mapping of LiMnO Electrodes Cycled in Lithium-Ion Batteries.
Buchberger D, Hamankiewicz B, Michalska M, Glaszczka A, Czerwinski A ACS Omega. 2024; 9(28):30381-30391.
PMID: 39035903 PMC: 11256290. DOI: 10.1021/acsomega.4c01480.
Zheng J, Xia R, Baiju S, Sun Z, Kaghazchi P, Ten Elshof J ACS Nano. 2023; 17(24):25391-25404.
PMID: 38088313 PMC: 10753873. DOI: 10.1021/acsnano.3c08849.
Ultraporous, Ultrasmall MgMnO Spinel Cathode for a Room-Temperature Magnesium Rechargeable Battery.
Kobayashi H, Fukumi Y, Watanabe H, Iimura R, Nishimura N, Mandai T ACS Nano. 2023; 17(3):3135-3142.