Controlled One-step Fabrication of Highly Oriented ZnO Nanoneedle/nanorods Arrays at Near Room Temperature
Overview
Authors
Affiliations
Highly oriented ZnO nanoneedle/nanorods arrays have been fabricated by direct oxidation of zinc foil in alkaline zincate ion solution at near room temperature (20 degrees C for nanoneedles, 30 degrees C for nanorods).
Wettability and Bactericidal Properties of Bioinspired ZnO Nanopillar Surfaces.
Zhang J, Williams G, Jitniyom T, Singh N, Saal A, Riordan L Langmuir. 2024; 40(14):7353-7363.
PMID: 38536768 PMC: 11008234. DOI: 10.1021/acs.langmuir.3c03537.
Interfacial Zinc Phosphate is the Key to Controlling Biocompatibility of Metallic Zinc Implants.
Su Y, Yang H, Gao J, Qin Y, Zheng Y, Zhu D Adv Sci (Weinh). 2019; 6(14):1900112.
PMID: 31380203 PMC: 6661942. DOI: 10.1002/advs.201900112.
Zhang X, Zhao H, Zhu Y, Yang Y, Jiang D, Chen X Regen Biomater. 2017; 4(4):223-231.
PMID: 28798868 PMC: 5544911. DOI: 10.1093/rb/rbx006.
Huang B, Shen P, Chen S Nanoscale Res Lett. 2010; 4(6):503-512.
PMID: 20596385 PMC: 2894128. DOI: 10.1007/s11671-009-9273-2.