Abstract

Statement Of Problem: One common test of single-unit restorations involves applying loads to clinically realistic specimens through spherical indenters, or equivalently, loading curved incisal edges against flat compression platens. As knowledge has become available regarding clinical failure mechanisms and the behavior of in vitro tests, it is possible to constructively question the clinical validity of such failure testing and to move toward developing more relevant test methods.

Purpose: This article reviewed characteristics of the traditional load-to-failure test, contrasted these with characteristics of clinical failure for all-ceramic restorations, and sought to explain the discrepancies. Literature regarding intraoral conditions was reviewed to develop an understanding of how laboratory testing could be revised. Variables considered to be important in simulating clinical conditions were described, along with their recent laboratory evaluation.

Conclusions: Traditional fracture tests of single unit all-ceramic prostheses are inappropriate, because they do not create failure mechanisms seen in retrieved clinical specimens. Validated tests are needed to elucidate the role(s) that cement systems, bonding, occlusion, and even metal copings play in the success of fixed prostheses and to make meaningful comparisons possible among novel ceramic and metal substructures. Research over the past 6 years has shown that crack systems mimicking clinical failure can be produced in all-ceramic restorations under appropriate conditions.

Citing Articles

Fracture resistance and mode of failure of modified Polyether-ether-ketone versus lithium disilicate endocrowns.

Kharboush M, Othman H, Aldamaty M, Alameldin A BMC Oral Health. 2025; 25(1):40.

PMID: 39773219 PMC: 11707867. DOI: 10.1186/s12903-024-05232-3.


Evaluating fatigue resistance in occlusal veneers: a comparative study of processing techniques and material thickness of lithium disilicate (IPS e.max Press vs. IPS e.max CAD).

Charoenporn W, Sornsuwan T, Sae-Lee D, Amornvit P, Chaijareenont P, Rungsiyakull P BMC Oral Health. 2024; 24(1):1542.

PMID: 39716117 PMC: 11665127. DOI: 10.1186/s12903-024-05347-7.


Fatigue behavior of sintered, glazed and glass-infiltrated surfaces of 5Y-PSZ bonded plates.

Carolina da Silva A, Ortiz L, Martins Alves L, Dapieve K, Campos T, Bottino M Braz Oral Res. 2024; 38:e027.

PMID: 39661784 PMC: 11654874. DOI: 10.1590/1807-3107bor-2024.vol38.0027.


The fracture resistance of pulpotomized primary molars restored with zirconia crowns, lithium disilicate or resin based ceramic endocrowns.

Ali A, Abo-Elsoud A, Helmy Y BMC Oral Health. 2024; 24(1):583.

PMID: 38764030 PMC: 11103835. DOI: 10.1186/s12903-024-04332-4.


Assessing the Efficacy of Novel Fiber-Reinforced Dual-Cure Luting Resins.

Lassila L, Garoushi S, Mangoush E, Vallittu P, Sailynoja E J Clin Exp Dent. 2024; 16(3):e333-e342.

PMID: 38600927 PMC: 11003287. DOI: 10.4317/jced.61396.